Abstract
The nanomechanical assessment of collagen fibrils via atomic force microscopy (AFM) is of increasing interest within the biomedical research community. In contrast to conventional nanoindentation there exists no common standard for conducting experiments and analysis of data. Currently used analysis approaches vary between studies and validation of quantitative results is usually not performed, which makes comparison of data from different studies difficult. Also there are no recommendations with regards to the maximum indentation depth that should not be exceeded to avoid substrate effects. Here we present a methodology and analysis approach for AFM cantilever-based nanoindentation experiments that allows efficient use of captured data and relying on a reference sample for determination of tip shape. Further we show experimental evidence that maximum indentation depth on collagen fibrils should be lower than 10–15% of the height of the fibril to avoid substrate effects and we show comparisons between our and other approaches used in previous works. While our analysis approach yields similar values for indentation modulus compared to the Oliver–Pharr method we found that Hertzian analysis yielded significantly lower values. Applying our approach we successfully and efficiently indented collagen fibrils from human bronchi, which were about 30nm in size, considerably smaller compared to collagen fibrils obtained from murine tail-tendon. In addition, derived mechanical parameters of collagen fibrils are in agreement with data previously published. To establish a quantitative validation we compared indentation results from conventional and AFM cantilever-based nanoindentation on polymeric samples with known mechanical properties. Importantly we can show that our approach yields similar results when compared to conventional nanoindentation on polymer samples. Introducing an approach that is reliable, efficient and taking into account the AFM tip shape, we anticipate that the present work may act as a guideline for conducting AFM cantilever-based nanoindentation of collagen fibrils. This may aid understanding of collagen-related diseases such as asthma, lung fibrosis or bone disease with potential alterations of collagen fibril mechanics.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: Journal of the Mechanical Behavior of Biomedical Materials
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.