ABSTRACT Fresh NR was adopted to prepare rubber with a nanomatrix structure. The nanomatrix structure was formed by graft-copolymerization of styrene onto deproteinized fresh NR (fresh DPNR) in the latex stage using tert-butyl hydroperoxide/tetraethylenepentamine as an initiator. Graft-copolymer consisting of fresh DPNR and polystyrene (fresh DPNR-graft-PS) was characterized by 1H-NMR spectroscopy and transmission electron microscopy. Under a suitable condition of the graft-copolymerization, conversion and grafting efficiency of styrene was 98 and 80 mol%, respectively. Morphology of fresh DPNR-graft-PS was observed by transmission electron microscopy. The rubber particles of about 1 μm in diameter were found to be dispersed in polystyrene matrix of 10–30 nm in thickness. Tensile properties of fresh DPNR were dramatically improved by forming the nanomatrix structure, compared with DPNR.