Abstract
In this study, the deformation behavior of single-crystal Si (100) was examined using nanoindentation, followed by analysis using cross-sectional transmission electron microscopy (XTEM), scanning electron microscopy (SEM), and Raman microspectroscopy. XTEM samples were prepared by focused ion beam (FIB) milling to accurately position the cross-section through the indentations. The deformation via phase transformation was clearly observed with micro-Raman and XTEM, showing the presence of high-pressure crystalline phases Si-III and Si-XII following pressure release. The indentation fracture toughness of Si is also discussed.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.