Abstract
Indentation tests and single-point scratch tests are probably the simplest methods of measuring the elastic, plastic and fracture behavior of brittle materials. In this paper, the nearsurface mechanical properties of KDP single crystal have been investigated including the elasticity like Young’s modulus E, and the plasticity like the hardness H. These material properties can be used to predict the material responses in optical manufacturing operations. Hardness and elastic modulus on different crystal plane of KDP single crystal have been examined under different loads by nanoindentation test, and the influence of the indentation load on hardness and elastic modulus have been also analyzed systematically. The results show the nanoindentation size effect, that is, the hardness and elastic modulus increase as the indentation load decreases. The hardness and elastic modulus have strong anisotropy in the different crystallographic orientation of the same crystal plane.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.