Abstract

The effect of laser shock peening (LSP) on mechanical properties of Ti-based bulk metallic glass (BMG) was investigated under nanoindentation. Two regions were generated within the specimen after the LSP: (I) the extremely thick softened region (∼300 µm) in which amounts of shear bands and excess free volume were generated; (II) the middle region where the free volume increased but nearly no shear bands were induced. The hardness decreased with the increase of the indenter depth (h), exhibiting indentation size effect (ISE). The ISE increased with the increase of the measured distance away from the laser shocked tip, indicating that the ISE was inhibited by the shear bands and excess free volume was generated by the LSP.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.