Abstract
ABSTRACTWe measure the mechanical response of optical multilayer dielectric (MLD) diffraction gratings, geometries which are constrained in only one transverse direction but free in the other, using nanoindentation. The results are explained using a stress-strain model, which reveals a uniaxial yield stress of 4.1- 4.6 GPa and predicts a similar dependence of yield stress on loads for both fully-elastic and fully-plastic solutions. Following R. Hill’s model of an expanding cavity under internal pressure, we show that the indentation response of the high-aspect ratio “pillar” geometry can be expressed in terms of uniaxial yield stress rather than material hardness.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.