Abstract
We report the experimental observations of buckling instabilities of vertical well-aligned single-crystal ZnO nanowires prepared on ZnO:Ga/glass templates. It was found that critical buckling load and buckling energy of the ZnO nanowires were 215 μN and 3.69×10 −11 J, respectively. It was also found that Young's modulus of the ZnO nanowires were 232 and 454 GPa while critical buckling strains were 0.35% and 0.18% when fixed–fixed column mode and fixed–pinned column mode were used, respectively.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: Physica E: Low-dimensional Systems and Nanostructures
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.