Abstract
Composite films of nano-size nickel grains embedded in a carbonaceous matrix are synthesized by a PVD process of C 60 fullerenes and Ni acetate. The morphology of the nano-composite films is characterized by TEM, selected area electron diffraction, chemical analysis and AFM. Correlations with deposition parameters and typical structure changes are found. The mechanical properties are analyzed by nanoindentation. The load–displacement charts show typical pop-ins correlated with the heterogeneous nano-structure. The depth dependent hardness and indentation modulus vary according to the nano-composite structure and reflect the changes of the mechanical properties in the film.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.