Abstract
"Nanoindentation mapping reveals gradients in the mechanical properties of dental enamel in rat incisors." Computer Methods in Biomechanics and Biomedical Engineering, 16(sup1), pp. 290–291Keywords:: rat dental enamelvariation in hardness and elastic modulusnanoindentation mapping AcknowledgementsB. Frýdová and V. Stejskal were supported by project VZ 0002700604 (Section 010). This research was also supported by the Technology Agency of the Czech Republic, grant no. TA01010185.