Abstract
We study the technique of nanoindentation hardness measurement applied to extremely hard and elastic thin films. We do the study with the aid of Hertz’s solutions for elastic contacts. The effect of different apical angles in ideally sharp conical diamond indenters is analyzed. In addition, the blunt tip shape of practical diamond indenters is discussed. The area function of the tip of real indenters is deduced from experimental nanoindentation measurements performed with these indenters on fused quartz. Triangular-base pyramidal indenters with Berkovich and cube corner geometries are considered. Theoretical hardness values applying Hertz’s and Oliver and Pharr’s methods of analysis are obtained and compared with the experimental data deduced from nanoindentation measurements performed on very hard and elastic ta-C films. The theoretical analysis shows a necessary dependence of the calculated hardness values with the apical angle of the indenter in totally elastic materials and to some extent in elastoplastic materials. Moreover, when the indenter tip is blunt or when there are inaccuracies in the measured area function of the indenter tip, hardness values decrease for very small penetration depths. Besides, in these films, because of their very small thickness, measured hardness values also decrease for measurements with penetration depths larger than a fraction of film thickness, due to the effects of the softer substrate.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: Applied Physics A Materials Science & Processing
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.