Abstract

The aim of this paper is to evaluate the microstructural and nanohardness characteristics of tungsten carbide-cobalt (WC-Co) cermet coatings deposited by liquid suspension spraying. Commercially available WC-Co coating powder was milled and water based suspension was produced as feedstock for the thermal spray coating process. Microstructural evaluations of WC-Co cermet coatings included XRD (X-Ray Diffraction) and SEM (Scanning Electron Microscopy). Post spraying nanomechanical evaluations were conducted using a Berkovich nanoindenter. Results indicated relatively higher modulus but lower hardness of suspension coatings. The load displacement curves during nanoindentation were characteristic of the complex coating microstructure showing signs of microcracking and pile-up.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.