Abstract
AbstractAsphalt concrete (AC) consists of coarse aggregate, asphalt binder, and fines. The asphalt binder creates an asphalt film around the coarse aggregate and fines. Fines are trapped inside the binder film, which is also known as mastic. Mastic and aggregate govern most of the mechanical properties of AC. Therefore, researchers have performed various tests on mastic to understand macroscale behavior of AC. Nanomechanical characterization is more appropriate for mastic, as the thinness of mastic is approximately 15–20 μm around an aggregate particle. For this paper, the authors conducted nanoindentation tests on mastic and aggregate as integral parts of AC. In particular, they compared the modulus and hardness of oven-aged mastic and aggregate with those of unaged mastic and aggregate. To deal with the heterogeneity of the mastic part, they made hundreds of indents on the mastic part of each AC sample. On the aggregate part, they made 60 indents to determine the mechanical properties of the aggregate o...
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.