In order to determine the effects of different mineral admixtures including fly ash (FA), blast furnace slag (BFS) and metakaolin (MK) on hydration product phases from the nanoscale structure perspective, nanoindentation characteristics of the samples with similar 28-day strengths have been investigated. The results indicate that the volume fractions of porosity in porosity and hydration product phases of the samples with the same kind of mineral admixture are almost equal to each other, and are greater than that of the sample without mineral admixture. Mineral admixtures especially MK can decrease remarkably the volume fractions of CH in porosity and hydration product phases, and there exists a good linear relationship between the (Al+Si)/Ca molar ratio of cementitious materials chemical compositions and the volume fraction of HD C-S-H gel in C-S-H gel. Therefore, it is possible to predict the volume fraction change of HD C-S-H gel in C-S-H gel by simply calculating the (Al+Si)/Ca molar ratio of cementitious materials with similar 28-day strengths under the constant water-binder ratio.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.