Abstract
In this research indentation instrument testing is used as a new method for local characterization to study different zones of friction stir welded AA6061 alloy. For this purpose nanoindentation and microhardness are applied for samples in as-weld and post weld heat treatment conditions. Nugget zone, thermomechanically affected zone, and heat affected zone are examined by using nanoindentor in both conditions. The observations say that an estimation of the truncated indenter tip defect is necessary because of pile-up. Whereas post weld heat treatment (PWHT) can recover elastic modulus and nanohardness as well as hardness in AA6061 weldment.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.