A new sulfonated SiO2 (S-SiO2) and sulfonated polystyrene ethylene butylene polystyrene (SSEBS) nanocomposite was used to fabricate a proton exchange membrane single chamber microbial fuel cells (SCMFCs). SSEBS containing various concentrations of S-SiO2 (2.5%, 5%, 7.5%, and 10%) was prepared. The nanomaterials and nanocomposite membranes were characterized by Fourier transform infrared spectroscopy, X-ray diffraction, scanning electron microscopy, and X-ray photoelectron spectroscopy. The nanocomposite membranes were also examined for their ion exchange capacity (IEC), water uptake, proton conductivity and oxygen crossover. The MFC with the SSEBS-S-SiO2 membrane (7.5%) exhibited a higher peak power density of 1209±17mWm−2 than other composite membranes. In the SSEBS and SSEBS-SiO2 membrane systems, the peak power density was 680±13mWm−2 and 852±11mWm−2, respectively. The composite membrane showed 4 times higher power density than the Nafion 117 membrane (290±7mWm−2). Overall, the composite membrane (particularly at S-SiO2 −7.5%) is a suitable technology in the MFC process because of its high proton conductivity imparted by S-SiO2.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.