Abstract

80 specimens of different microstructure were prepared from arc-welded steel plates, which were welded with mildsteel, 1.5%Cr-Mo steel, 5%Cr steel, 13%Cr steel and 18Cr-8Ni steel deposited metals, under the adequate welding conditions. The mechanical properties of specimens and their defects were inspected by means of X-ray and supersonic waves.Then, the loss by corrosion, volume of hydrogen produced, and their electrode potential in 10% H2SO4, HCl, at the welded and annealed states, were measured. Welded strain was also studied.The results are as follows;1) The corrosion loss, and fuming hydrogen volume are changed remarkably according to the microstructure.2) It is not so efficient to use 1.5%Cr-Mo steel as the deposited metal for corrosion prevention.3) It is natural that the corrosion resistance of bead part is much increased when 18-8 steel is used as the deposited metal.4) The corrosion resistance of high sulphur mild steel plate is low as compared with low sulphur mild steel plate.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.