Studies were made on the blisters which appear on the plated surface of zinc alloy die castings after several months more since the plating. The processes for accelerating the appearance of these blisters were also discussed. The following results were obtained(1) Each blister had a circular gap of 30-40μ in dia. at its centre, from which cracks radiated.(2) Growth of blisters was due to the corrosion of the substratum of zinc alloy.(3) For accelerating the appearance of blisters, it was found to be most effective to immerse the castings in the solution of about 3% of NH4Cl in boiling.(4) The blisters appeared in the above test were considered to be the same in nature as that in practice. Accordingly, the above test would be most available for detecting the surface defects for blistering source.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.