Abstract
By the SHS reaction of mechanically alloyed Al-Ti powders set on Cu surface, thick and homogeneous Al3Ti layer free from unreacted elements was prepared in order to improve the wear properties of Cu. The surface layer was chemically binded with base metal by the formatin of three reaction layers. To prepare the MA powders for SHS reaction, it was comfirmed that MA time should be optimized because too short length of MA leads to the existance of unreacted elements. Furthermore, too long length of MA decreases the heat of reaction due to the formation of Al super saturated solid solution during MA.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: Journal of the Society of Materials Science, Japan
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.