Abstract
For each matrix powder size, the tensile strength of composite increased proportionally with increasing volume fraction of the whisker, Vf, up to a critical value, (Vf)c, beyond which the strength was holded. (Vf)c increased with decreasing powder size. Thus, the composite produced with finer matrix powder was effectively strengthened by the whisker up to higher Vf. The amount of whisker per unit surface area of matrix powder calculated for each size of powder at (Vf)c coincided approximately with each other. The specific amount of whisker was considered to be a limitation to effectively reinforce the matrix. As for the effect of heat treatment on the strength of composite, it was 20% increased by heating at 913 K for about 30ks. On the other hand, the prolonged heat treatment reduced the strength by causing remarkable reaction between the whisker and the matrix.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.