Abstract
This paper presents some experimental results of single crystal ferrite in scratch tests with various shapes of diamond chisels and in grooving tests with diamond wheels.On scratch tests with diamond chisels, there is no crack on the surface of a groove but plastic flow is generated at a small scratch load less than 0.02-0.05 N. The height of plastic flow is as large as the depth of a groove. On the other hand, such small plastic flow, called as burr, as about 0.1 μm high and 1, μm wide, is created on both shoulders of grooves in groove grinding of single crystal ferrite using diamond wheels. The burr height has a strong correlation with the uncut chip thickness which is determined by such factors as wheel speed, table speed, depth of cut and the amplitude of forced vibration of a wheel. For restraining the burr height, keeping the small uncut chip thickness on each cutting edge of grains are recommended.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: Journal of the Japan Society for Precision Engineering
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.