Abstract
In shearing process, such as blanking or piercing on the sheets of both aluminum and magnesium alloys, there are problems that large burrs generate and the accuracy of cut surface is worse after a few repetitions of these processes. Therefore, in this study, we investigated the cause and solution of these problems. We found that the cause was not the deterioration of the tool edge due to wear or chipping, but that materials of the sheared sheets which adhered to the side of the tool shaved the cut surfaces of the sheets during shearing or adhered to the cut surfaces and induced partial plastic deformation. We also found that a hard-carbon-film-coated tool is effective in preventing the generation of adhesive materials, thereby preventing both the generation of large burrs and the decrease in the accuracy of cut surfaces.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.