Abstract

Influence of silicon and niobium on weldabilities of ferritic stainless steel welding wire have been investigated. The results are as follows. (1) At MIG and MAG welding, the weld cracking proof characteristic was improved by the addition of 1.0% silicon to weld wire and decreasing the niobium content of weld wire to 0.2%. (2) The developed weld wire with copper coating is excellent in the flatness of weld bead and the corrosion resistance.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.