The purpose of this in vitro study was to compare the dimensional accuracy of maxillary dentures made using a conventional heat-activated PMMA resin, a pour resin, a visible light-activated resin, and a microwave-activated acrylic resin. Two simple methods for measuring dimensional accuracy were used: (1) weight of impression material entrapped between the base and master die and (2) measurement of the posterior border gap at five locations. The volume of space between the denture base and the master die was determined by (1) computation and (2) estimation. Statistical analysis (Bartlett, ANOVA and Tukey's Tests) supported the following conclusions: (1) all groups showed a processing contraction, most apparent from buccal flange to buccal flange, (2) the poorest fitting group was processed in a brass flask and a water bath at a temperature which rose from 70 to 100 degrees C, using a heat activated resin (Acron), (3) the visible light activated resin (Triad) produced dentures of intermediate accuracy, as did Acupac 20 when either heat or microwave activated, (4) the two best fitting groups were prepared from a chemically activated resin system using pressure at low heat (PER form), and the resin developed for microwave activation (Acron MC).

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.