Lanthanum chromites ((La, A) (Cr, M) O3; A=Ca, Sr, M=Co, Ni, Cu, Zn) were synthesized and characterized from their density, thermal expansion coefficient and chemical stability. Cobalt doped lanthanum calcium chromites with La-site/Cr-site ratio>1 were densely sintered at 1400°C, and it is possible to adjust the thermal expansion coefficient to that of YSZ by controlling the amount of dopants. Lanthanum strontium chromites with La-site/Cr-site ratio=1 were not densely sintered at lower temperature than Ca-doped, but kept enough strength after reduction treatment. difference of strength change after the reduction treatment between Sr-doped and Ca-doped ones is related to the difference in lattice expansion after the treatment.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.