Abstract
Production lapping of lead zirconate-titanate ceramics are dealt with lapping rate, parallelism, yield and machining time including cutting-off time, since ceramics are machined as planeparallel, slender, thin plates in using for relay switches. The results obtained are as follows : (1) The order in lapping rate is A (no additive) >D (added Cr) >C (added Nb) >B (added Fe). Strong specimen C has a yield of 95%. (2) The difference in plate thickness within 10μ and the parallelism of 2μ are obtained from plane-parallel lapping, where the motion of specimens is restricted in carriers. (3) The concentration of lapping vehicle influences on lapping rate only by a factor of 5%. Supplying vehicle at a rate of 150 cc/min is desirable for preventing from breakage of plates. (4) Cut-off thickness is chosen as 0.3 mm regardless of the kind of ceramics. The whole machining time in lapping plates of 0.3 mm thick to 0.2 mm thick is shortened by a factor of about 40% than in lapping plates of 0.5 mm thick.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: Journal of the Japan Society of Precision Engineering
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.