Abstract

Thixoforming involves processing alloys with a spheroidal microstructure in the semisolid state. Commercially it is applied to conventional casting alloys, and one of the scientific challenges is to extend its application to high performance aluminium alloys such as 7075. Aluminium alloy 7075 is readily available in extruded form, and one route to a spheroidal microstructure is to reheat extruded material into the semisolid state to obtain recrystallisation, with the liquid penetrating the recrystallised boundaries. Here this route has been followed, but it has been found that the presence of pinning particles in the microstructure inhibits recrystallisation. To overcome this, a multistep induction heating regime has been developed consisting of a 1 min hold at 475-500 °C, a 1 min hold at 575-600 °C and a shorter 20 s hold for the final step at 620 °C.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.