Abstract
In this study, a multi-scale model that integrates a macro-scale transient three-dimensional mass and heat transfer model and a micro-scale thin-interface phase-field model is developed to simulate the solidification behavior of the molten pool and the dendritic growth behavior for direct energy deposition process. Both the longitudinal molten pool morphology and the primary dendritic arm spacing (PDAS, Λ) of the columnar dendrites are validated by experiments. As revealed from the macro-scale simulation, the solidification velocity Vs and the temperature gradient G are coupled with an opposite trend, and the cooling rate R decreases along the solid/liquid interface from the top to the bottom of the molten pool. The micro-scale simulation shows that a power-law function (Λ ∝ R−1.31) with a scaling factor much larger than a traditional directional solidification (Λ ∝ R−0.5). Moreover, contrary to Hunt's and Kurz-Fisher's linear models, a circuitous relationship between Λ and G−0.5Vs−0.25 is found to be clustered within a narrow region. The coupled solidification parameters along the solidification interface with an asymptotic increase of G near the bottom of the molten pool contribute to the above PDAS observations.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.