Abstract
A multiscale simulator for alumina film growth inside a nanoporous material during an atomic layer deposition process is developed. The model combines a continuum description at the macroscopic level of precursor gas transport inside a nanopore during exposure to each of the two precursor species (trimethyaluminum and water) with a Monte Carlo simulation of the film growth on the microscopic scale. Simulation results are presented for both the Monte Carlo simulation and for the multiscale system, the latter illustrating how nonuniform deposition along the nanopore can occur when insufficient precursor exposure levels are used.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.