Abstract
Mutlifrequency parametric Raman generation was carried out in a KGd(WO(4))(2) crystal by use of a dual-wavelength Ti:sapphire laser system. It was found that with femtosecond pump pulses the efficiency of Raman generation is low because of the onset of self-phase modulation. The mechanism for suppression of stimulated Raman scattering by self-phase modulation is discussed. Employing 2-ps-long chirped pulses generated four Stokes and one anti-Stokes component.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.