Abstract

Wheel tracking testing on AC-20 limestone asphalt mixtures was carried out to determine the effect of multi-stress loading on rutting development. Rutting rates increased with the application of higher levels of stress, however, they reduced with the subsequent application of lower stresses. The primary densification rates were highest in the first loading phase, after which rutting development became solely dependent on the secondary rutting rates. 50°C was the shift temperature for rutting development, below which rutting rates increased linearly, but the increase became exponential at higher temperatures. Heavier loads applied first caused accelerated damage, but their effect was minimised when lighter stresses were applied beforehand. A rutting index based on a new multi-stress analytical model was proposed, and could be used to evaluate the rutting performance of mixtures under more realistic loadings.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.