The thermal decomposition of alkali (Li,Na,K,Cs,NH 4) tris(oxalato)ferrates(III) has been studied at different temperatures up to 700°C using Mössbauer, infrared spectroscopy, and thermogravimetric techniques. The formation of different intermediates has been observed during thermal decomposition. The decomposition in these complexes starts at different temperatures, i.e., at 200°C in the case of lithium, cesium, and ammonium ferrate(III), 250°C in the case of sodium, and 270°C in the case of potassium tris(oxalato)ferrate(III). The intermediates, i.e., Fe 11C 2O 4, K 6Fe 11 2(ox) 5. and Cs 2Fe 11 (ox) 2(H 2O) 2, are formed during thermal decomposition of lithium, potassium, and cesium tris(oxalato)ferrates(III), respectively. In the case of sodium and ammonium tris(oxalato)ferrates(III), the decomposition occurs without reduction to the iron(II) state and leads directly to α-Fe 2O 3.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.