The influence of a few percent neodynium additives to Fe-B alloy on the hyperfine parameters was investigated. It was found that Nd decreases the hyperfine field of amorphous Fe-B alloys. The samples annealed at temperatures between 600°C and 700°C contain α-Fe and Fe3B phases. The average hyperfine field of Fe3B phase increases with increasing Nd content and decreases with increasing annealing temperature. The average isomer shift of Fe3B phase decreases with increasing Nd content. The experimental data show that the change of hyperfine parameters of the Fe3B phase in the studied alloys is due to Nd atom.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.