Abstract

Double and triple crystal rocking curve and peak position maps are constructed for a 4HSiC wafer for the symmetric (0 0 0 8) reflection in the normal position, the same reflection for a sample rotated 90º, and an asymmetric (1 23 6) reflection for the wafer in the normal position. These measurements were corrected for the ‘wobble’ in the instrument by scanning a 4” (1 1 1) Si wafer and assuming that the Si wafer was perfect and attributing the variations in the measurements to instrumental error. The x-ray measurements are correlated with a cross polar image, etch pit density map, white beam transmission x-ray topograph, and a laser light scan.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.