Abstract

Uranium and uranium–zirconium electrodeposits produced in the Fuel Cycle Facility at Argonne National Laboratory-West were examined using standard metallurgical techniques. Substantial differences in the morphologies of the two types of deposits were observed. Samples from pure uranium deposits were comprised of chains of uranium crystals with a characteristic rhomboidal shape, while the morphologies of samples from deposits containing zirconium in excess of approximately 0.5 wt% showed more polycrystalline features. Zirconium was found to be present as a second, zirconium metal phase at or very near the uranium–zirconium dendrite surfaces. Higher collection efficiencies and total deposit weights were observed for the uranium–zirconium deposits; this performance increase is likely a result of better mechanical properties exhibited by the uranium–zirconium dendrite morphology.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.