Abstract

Electrical calcium (Ca) test was used to measure water vapor transmission rate (WVTR) through polyimide (PI) substrate with barrier films. The WVTR was obtained by measuring the resistance of the Ca as a function of time. Barrier films consisted of silicon oxide (SiOx)/silicon nitride (SiNx) stacks were consecutively deposited onto the PI substrate at 350°C by plasma-enhanced chemical vapor deposition. SiNx and SiOx films show great moisture impermeability while the SiNx film presented higher moisture resistance than the SiOx film. The sample of PI coated with SiOx/SiNx stacks was kept flat by stress compensation of SiNx film and SiOx film. The WVTR value of the optimum barrier structure (5 pairs of SiOx/SiNx) is 5.58×10−6g/(m2day) under an electrical Ca test (25°C, 40% relative humidity). After 500 times cyclic bending in a compressive mode, WVTR value keeps below 4.32×10−5g/(m2day). The SiOx/SiNx barrier stacks presented on PI have a great potential for flexible electronics applications.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.