Abstract
The development of piezoelectric ceramics with large piezoelectric coefficient (d33), high Curie temperature (Tc) and high mechanical quality factor (Qm) is still a key challenge for practical application for high-power device. Herein, a series of Sm3+ and Mn2+ ions co-doped 0.15Pb(Mg1/3Nb2/3)O3-(0.85-x)PbZrO3-xPbTiO3 ceramics were prepared by the solid-state sintering method. The optimum piezoelectric properties were achieved at x = 0.435 mol% with a large d33 ∼ 450 pC/N and a high Qm ∼ 1968 near the morphotropic phase boundary (MPB), and with high Tc ∼ 296 °C. The origin of this excellent piezoelectric properties was explained by the phase structure, piezoelectric and dielectric analysis. The composition near MPB region and the appearance of defect dipoles leaded to final excellent piezoelectric properties, and made a harmonization between d33, Tc and Qm. This work demonstrated a rational strategy to obtain large d33, high Tc and high Qm for high-power piezoceramics.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.