Abstract

Nowadays, The Nuclear Power Plant (NPP) Lifetime can be extended to around 80 Years; This Is Assist to Recommend the Modifications Some Properties of Polymeric Cross Linked Polyethylene (XLPE) Cable Insulation. This Work is A Laboratory Implementing the Nano-fillers as Silicon Dioxide (Sio2) and Clay to Enhance Cable Insulation. The Volume Resistivity, Capacitance, Dielectric Loss, Tensile Strength and Elongation Properties Were Tested and Measurement for the Nanorized Samples. Furthermore, These Measurements Have Been Carried Out for the (XLPE) with Modified XLPE/Sio2 and XLPE/Clay, at Additive Concentration of 1, 2.5, 4 and 5 Weight Percentage (Wt%). The Officially Documented Results Have Been Provided Much Better Cable Electrically Insulation and Mechanically Profile. A 205% and 189% for Volume Resistivity and Instance were improved for The XLPE/Sio2 and XLPE/Clay Respectively, and The Analytical Calculations were in Agreement with the Experimental Results.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.