Abstract

The purpose of this study was to evaluate the performance of modified 4-META/MMA-TBB resin cements (Superbond C&B) in terms of debonding orthodontic brackets easily and safely from enamel without the loss of proper bracket bond strength. Poly (DL-lactide-co-glycolide) (PLGA), calcium fluoride (CaF2), or alpha-tricalcium phosphate (alpha-TCP) was added to the polymer powder of 4-META/MMA-TBB resin, and the shear bond strength of orthodontic brackets to human enamel using modified resins was measured before and after 10,000-cycle thermal cycling test between 5 degrees C and 55 degrees C. The modified resins tended to provide lower bond strength compared with the original 4-META/MMA-TBB resin. However, alpha-TCP- or CaF2-modified resin showed no significant differences in bond strength before and after thermal cycling. Moreover, there was a tendency of more residual resin remaining on the tooth surface after debonding, thereby suggesting a lower risk of enamel fracture. In conclusion, alpha-TCP- or CaF2-modified 4-META/MMA-TBB resin seemed to allow easy and safe debonding of orthodontic brackets without loss of proper bracket bond strength.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.