Abstract
The development of advanced Ni-based superalloys for gas turbine applications is strongly reliant on alloy strength design and optimisation through microstructure control. Herein, a new model of precipitation strengthening in Ni-based superalloys with large amounts of cuboidal γ’ particles is proposed and directly validated using commercial alloy (Alloy720Li)-based single-crystal tie-line model alloys with specially designed γ’ particle sizes and volume fractions. All factors responsible for Ni-based superalloy strengthening, including the γ/γ’ mixture, particle strengthening, and solid solution strengthening are extracted from the compressive stress-strain curves performed over a wide temperature range. The strength increment due to particle strengthening is predicted for five model alloys with various γ’-particle volume fractions, sizes, and shapes. The pair-coupling model assuming the presence of cuboidal γ’ particles accurately predicts alloy strength over a wide temperature range (up to 760 °C) for volume fractions of >45%, whereas the classical model assuming spherical γ’ particles is valid only for volume fractions of <20%. Thus, the former model is much more accurate than classical models across wider volume fractions up to the disc service temperature, contributing to the design of further strengthened superalloys.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have