Abstract
In this paper the TMF crack initiation behaviour of the single-crystal nickel-base superalloyMD2 is investigated and modelled. TMF tests were performed in both IP and OP for varying mechanicalstrain ranges in the [001] crystallographic direction until TMF crack initiation was obtained. Acrystal plasticity-creep model was used in conjunction with a critical-plane approach, to evaluate thenumber of cycles to TMF crack initiation. The critical-plane model was evaluated and calibrated ata stable TMF cycle, where the effect of the stress relaxation had attenuated. This calibrated criticalplanemodel is able to describe the TMF crack initiation, taking tension/compression asymmetry aswell as stress relaxation anisotropy into account, with good correlation to the real fatigue behaviour.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.