The thermal oxidation behaviour of polyethylene films stabilized by various weight ratios of organophosphites (Irgafos 168) has been studied at selected temperatures. The duration of the induction period was found to increase proportionally with the stabilizer concentration, even at temperatures as low as 80 °C. Particular attention was paid to the phosphite–phosphate conversion during the induction period. A kinetic model, involving volatile and partially soluble hydroperoxide decomposers, was developed in order to simulate these results. With the use of kinetic parameters that can be at least tentatively justified from theoretical considerations, this model gave simulations in reasonable agreement with the experimental observations for stabilizer depletion and carbonyl formation. Of particular note is the fact that, even for non-trivial results such as the shape of the phosphite versus phosphate concentration plots, or phosphate build-up, there was also a quite good agreement.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.