Abstract

ABSTRACTFinite‐element predictions of creep rupture in notched specimens are presented in this work. A damage model linked to the creep strain rate and stress triaxiality has been used to predict creep life under multiaxial stress conditions and the predictions have been compared with experimental data for a C–Mn steel. Finite‐element analyses have been conducted using primary–secondary (PS) and primary–secondary–tertiary (PST) creep laws. As expected a PST analysis gives a shorter predicted rupture life than a PS analysis. An additional term was included in the model to allow for an increase in hydrostatic strain due to creep damage. The incorporation of this term improved the agreement between the experimental data and the finite‐element predictions. A further enhancement to the model was to model the initiation and growth of a sharp crack in the vicinity of the notch, through the use of a nodal release technique linked to the damage evolution. It was found that the predictions obtained using the nodal release technique were very similar to those from the PST creep model incorporating the hydrostatic damage term. The effect of mesh size has also been examined and the finite‐element predictions were seen to be quite mesh sensitive with a finer mesh generally giving a shorter predicted life.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.