Abstract
Abstract A model has been developed to predict internal pitting corrosion of oil and gas pipelines. This model is based on experiments carried out in the laboratory at high pressure and high temperature under the operating conditions of the oil and gas pipelines. There are two kinds of inputs: construction (pipe diameter, pipe wall thickness, and pipe inclination) and operational (production rates of oil, water, gas, solid, temperature, total pressure, partial pressures of hydrogen sulfide [H2S] and carbon dioxide [CO2], concentrations of sulfate, bicarbonate, and chloride). The model accounts for the statistical nature of the pitting corrosion, predicts the growth of internal pits based on the readily available operational parameters from the field, includes the pit growth rate driven by variables not included in the model, considers the variation of the pitting corrosion rate as a function of time, and determines the error in the prediction. The validity of this model was checked using data obtained fro...
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.