Abstract
It is widely believed that the activities of bone cells at the tissue scale not only govern the size of the vascular pore spaces (and hence, the amount of bone tissue available for actually carrying the loads), but also the characteristics of the extracellular bone matrix itself. In this context, increased mechanical stimulation (in mediolateral regions of human femora, as compared to anteroposterior regions) may lead to increased bone turnover, lower bone matrix mineralization, and therefore lower tissue modulus. On the other hand, resorption-only processes (in endosteal versus periosteal regions) may have the opposite effect. A modal analysis of nanoindentation data obtained on femurs from the Melbourne Femur Research Collection (MFRC) indeed confirms that bone is stiffer in endosteal regions compared to periosteal regions (E̅endost = 29.34 ± 0.75 GPa >E̅periost = 24.67 ± 1.63 GPa), most likely due to the aging-related increase in resorption modeling on endosteal surfaces resulting in trabecularization of cortical bone. The results also show that bone is stiffer along the anteroposterior direction compared the mediolateral direction (E̅anteropost = 28.89 ± 1.08 GPa >E̅mediolat = 26.03 ± 2.31 GPa), the former being aligned with the neutral bending axis of the femur and, thus, undergoing more resorption modeling and consequently being more mineralized.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: Journal of the Mechanical Behavior of Biomedical Materials
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.