Abstract
Blends of poly(oxybenzoate-p-ethylene terephthalate) (POB-PET) and polyarylate were confirmed to be a partially miscible system by differential scanning calorimetry. When 60/40 POB-PET/PAr blend was annealed at high temperature (above 270°C) for several minutes, the ester–ester interchange (transesterification) in the blend took place immediately, as evidenced by Fourier Transformed infrared analyses. The analysis of the blend annealed at 290°C by 1H-13C nuclear magnetic resonance disclosed that there were four new diads appearing in 15 min and an additional one produced in 60 min during the heat treatment. The miscibility between POB-PET and polyarylate increased with the mol concentration of these new diads judging from differential scanning calorimetry. The evolution of the concentration of the diad ethylene glycol-isophthalate during the annealing can be described by a second-order reaction. The activation energy of forming the diad ethylene glycol-isophthalate was 26.5 kcal/mol, and the preexponential factor for the transesterification reaction is 3.7 × 108 min−1. © 1998 John Wiley & Sons, Inc. J Polym Sci B: Polym Phys 36: 1959–1969, 1998
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: Journal of Polymer Science Part B: Polymer Physics
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.