AbstractThe effects of the surface energy, storage modulus (G′), and glass‐transition temperature (Tg) on the biofouling behavior of siloxane and fluorosiloxane polymer surfaces (films) were studied. Irregular SiH‐terminated tetrabranched star oligosiloxanes and star oligofluorosiloxanes were prepared by the acid‐catalyzed equilibration of octamethylcyclotetrasiloxane or 1,3,5‐trimethyl‐1,3,5‐tris(3′,3′,3′‐trifluoropropyl)cyclotrisiloxane with tetrakis(dimethylsiloxy)silane, respectively. Terminal epoxy groups were introduced via Pt‐catalyzed hydrosilylation with allyl glycidyl ether to yield compounds that were subsequently crosslinked with α,ω‐bis(3‐aminopropyl)poly(dimethylsiloxane). The resulting films were characterized by goniometry, dynamic mechanical thermal analysis, and thermogravimetric analysis. The foul‐release behavior was studied by the measurement of how strongly sporelings (young plants) of the green seaweed Ulva adhered. The corrosion protection of aluminum was evaluated by electrochemical impedance spectroscopy. Fluorosiloxane films displayed higher G′ and Tg values, decreased contact angles (with water), and more effectively released Ulva sporelings in comparison with siloxane films. © 2006 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 44: 2551–2566, 2006

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call