Abstract

This study reports the physicochemical analysis of three alluvial clastic clays from the Ngaye River in northern Cameroon. X-ray diffraction, infra-red spectroscopy, scanning electron microscopy and thermal analysis are used to establish the mineralogical composition. It is found that the main clay minerals in these samples are kaolinite, muscovite-illite and smectite associated with quartz, goethite, feldspars and anatase. This mineralogical assemblage is in accordance with the chemical analysis which further confirmed the high quartz proportion. The low content in fluxing agent is indicated by the low contents in Na2O, K2O, MgO and CaO. The low content in fluxing agent and high sand proportion result in poor vitrification in ceramic testing brick obtained at 900 °C, 1000 °C and 1100 °C. For all the firing temperatures, linear shrinkage varied from 0.7% to 2.6%, weight loss varied from 3.5% to 7%, bulk density varied from 1.6 to 1.8 g/m3, water absorption decreased from 20.7% to 12.7%, and flexural strength (σ) varied from 0.60 to 2.07 MPa.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.