Abstract

Experiments have been conducted with Huolinhe lignite low temperature ashes (HLH-LTA) to investigate the mineral behaviors under gasification atmosphere (H2/CO2=1:1, volume ratio) with the temperature increase by SEM and XRD. The results show that the contents of SO3 and alkali metal oxide (e.g. K2O, Na2O) are higher in the HLH-LTA than that in laboratory HLH ashes. The formation of some low-melting ferrous eutectic compounds causes the initial melting temperature of HLH-LTA is lower about 300 °C than its deformation temperature. The formation of slag during HLH fluidized-bed gasification is the results of the interaction among minerals and phase changes with the temperature increases under reducing atmosphere.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.