Abstract

We are presenting data for polyethylene, polypropylene, poly-4 methyl pentene-1 (TPX), polytetrafluorethylene, plexiglass, acrylic and nylon over the frequency range 50–300 GHz., The first four are non-polar and exhibit extremely low loss characteristic. The last three are typical polar polymers but exhibit nearly twenty to thirty times higher loss than polar-polymers.