Abstract

Microwave-enhance catalytic degradation (MECD) of 4-chlorophenol (4-CP) using nickel oxide was studied. A mix-valenced nickel oxide was obtained from nickel nitrate aqueous solution through a precipitation with sodium hydroxide and an oxidation by sodium hypochlorite (assigned as PO). Then, the as-prepared PO was irradiated under microwave irradiation to fabricate a high active mix-valenced nickel oxide (assigned as POM). Further, pure nanosized nickel oxide was obtained from the POM by calcination at 300, 400 and 500 °C (labeled as C300, C400 and C500, respectively). They were characterized by X-ray (XRD), infrared spectroscopy (IR) and temperature-programmed reduction (TPR). Their catalytic activities towards the degradation of 4-CP on the efficiency of the degradation were further investigated under continuous bubbling of air through the liquid-phase and quantitative evaluation by high pressure liquid chromatography (HPLC). Also, the effects of temperature, pH and kinds of catalysts on the efficiency of the degradation have been investigated. The results showed that the 4-CP was degraded completely by MECD method within 20 min under pH 7, T = 40 °C and C = 200 g dm −3 over POM catalyst. The relative activity was affected significantly with the oxidation state of nickel.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.